Reordering a diaphragm usually comes down to one line on the form: PTFE, Santoprene, Hytrel, Buna-N, etc. Get it wrong, and a diaphragm pump that should run for months or years can split the diaphragm in weeks, or worse, an incorrect elastomer can swell or fail the first time it meets a solvent.
As an official Graco distributor in New Zealand, we answer this question often. Here’s how the materials compare, when a PTFE diaphragm pump is worth the extra cost, and a chemical chart to check before you reorder.
In AODD pumps (air-operated double diaphragm pumps), the diaphragm flexes on every stroke. It’s also the only barrier between your process fluid and the pump’s air side motor.
When the diaphragm material doesn’t suit the fluid, it can swell, harden, or crack. Fluid can then enter the air side, contaminate product, and stop production without warning. The diaphragm is one of the cheapest parts in the pump, but it often decides how much downtime you’ll have.
PTFE (polytetrafluoroethylene) is the go-to material for aggressive fluids. Graco rates it as the most chemically compatible diaphragm material it offers, with extreme corrosion resistance and a low-friction, non-stick surface. If you’re moving concentrated acids, solvents, or strong caustics, the conversation usually starts with a PTFE diaphragm pump.
But PTFE has trade-offs. It isn’t an elastomer, so it’s stiffer than rubber and less forgiving of constant flexing. That’s why standard PTFE diaphragms run with a backer diaphragm behind them.
A two-piece PTFE diaphragm pairs a PTFE face with a separate backer. Graco’s overmoulded PTFE bonds an FDA-compliant PTFE face and an EPDM air side into one part, with no exposed diaphragm plate on the fluid side. Graco reports up to three times longer diaphragm life with overmoulded PTFE on its ½” to 3″ pumps compared with standard diaphragms.
Its maximum temperature is lower at 82°C, although it handles colder conditions down to -10°C. Check your process temperature before you switch. For sites pumping slurries or pigmented fluids that still need PTFE, fewer change-outs mean less downtime and lower labour costs across the year.
Here’s how PTFE compares with other diaphragm materials in Graco’s range. These temperature limits are based on mechanical stress only, so some chemicals will narrow them further.
Graco Diaphragm Materials Compared:
| Material | Temperature Range | Strengths | Watch Out For |
| PTFE | 4°C to 100°C | Widest chemical compatibility, non-stick | Poor abrasion resistance, needs a backer |
| Overmoulded PTFE | -10°C to 82°C | PTFE chemistry with longer life in abrasive duty | Lower maximum temperature |
| Santoprene | -40°C to 82°C | Abrasion and chemical resistance; caustics, dilute acids, alcohols, some solvents | Concentrated chemicals usually need PTFE; petroleum oils |
| TPE (Hytrel) | -29°C to 66°C | Low-temperature performance, abrasion resistance | Lowest top temperature in the range |
| G.E.T. (Graco Engineered Thermoplastic) | -40°C to 82°C | Abrasion resistance, similar chemistry to Buna-N | Strong solvents |
| Buna-N (nitrile) | -12°C to 82°C | Petroleum fluids, oils, water | Acetone, MEK, chlorinated solvents |
| EPDM | -51°C to 135°C | High heat, steam, caustics, CIP sanitisers | Petroleum oils |
| FKM (Viton) | -40°C to 160°C | High heat, acids, fuels | Ketones, low molecular weight esters |
Graco’s own popular configurations pair TPE with *petroleum products on aluminium pumps and Santoprene with diluted chemicals on polypropylene pumps. PTFE takes over once the chemicals get concentrated.
*Unleaded Fuel
Most PTFE chemical compatibility chart pages online come from lab suppliers and rate a static sample soaked for 48 hours. A diaphragm flexes thousands of times a shift, so use the PTFE chemical resistance chart below as a starting point. Then confirm against Graco’s Chemical Compatibility Guide for your exact concentration and temperature.
| Fluid (Typical NZ Use) | PTFE | Santoprene | Buna-N | EPDM | ||
| Caustic soda (dairy CIP) | ✓ | ✓ | ~ | ✓ | ||
| Dilute acids | ✓ | ✓ | ~ | ✓ | ||
| Concentrated acids | ✓ | ~ | ✗ | ~ | ||
| Sodium hypochlorite (wastewater dosing) | ✓ | ~ | ✗ | ~ | ||
| Peracetic acid sanitiser, e.g. Oxonia (food CIP) | ✓ | ~ | ✗ | ~ | ||
| Ketones such as MEK and acetone (coatings) | ✓ | ~ | ✗ | ✓ | ||
| Diesel, oils, and petroleum fluids | ✓ | ✗ | ✓ | ✗ | ||
This is for general guidance only. Confirm with Graco’s Chemical Compatibility Guide or our team before ordering.
One more thing. A PTFE diaphragm won’t protect an incompatible ball, seat, or O-ring. Graco’s rule is to stay within the limits of the most restricted wetted part, so check the whole pump. PTFE itself is attacked by only a handful of chemicals, such as molten alkali metals like sodium and fluorinating agents.
If you’ve searched for a PFA vs PTFE chemical resistance chart, here’s the short answer: chemically, they’re almost identical. Both are fluoropolymers rated as inert to nearly all industrial chemicals.
The difference is in how they’re made and how they flex. PFA can be melt-processed, which suits moulded linings, fittings, and tubing. PTFE handles repeated folding better, and that’s exactly what a diaphragm does all day. So your pump runs a PTFE diaphragm, while PFA is more likely to turn up in lined pipework.
| Property | PTFE | PFA |
| Chemical resistance | Inert | Inert |
| Melt-processable | No | Yes |
| Diaphragm flexing | Better suited to continuous flexing | Good, but rarely used for diaphragms |
| Heat resistance | Slightly higher | Slightly lower |
| Typical pump-system use | Diaphragms, check balls | Linings, fittings, tubing |
Swelling, cracking around the bolt holes, or fluid in the air exhaust all signal that the material isn’t right for your duty. A cheaper look-alike rarely fixes it. Our guide to genuine Graco parts explains why non-genuine diaphragms end up costing more.
Our in-house team can review your fluid, build a preventive maintenance plan around it, and keep the right diaphragm kits on hand. Ask us about our current stock of Graco diaphragm kits when you need a replacement.
For concentrated or aggressive chemicals, yes. For diluted chemicals, water, and abrasive fluids, Santoprene often lasts longer and costs less.
Graco rates standard PTFE from 4°C to 100°C and overmoulded PTFE from -10°C to 82°C, before any chemical limits apply.
Often, yes, if a kit exists for your model. Check the balls, seats, and O-rings too, since they need to suit the fluid as well.
Send us your fluid, temperature, and pump model, and we’ll confirm the right diaphragm and dispatch genuine Graco parts. Specifying a whole new pump instead? Compare AODD vs EODD pumps first, as Graco’s electric diaphragm pumps can cut energy costs by up to 80% compared with air-operated models.
Address: 16/10 Olive Road, Penrose, Auckland 1061
Phone: 0800 215 104
Email: [email protected]